Hi, I’ve tried to print a model plane for my father. It’s this model, using this LW-PLA right after purchase.

As you can see in the image of this post, the print is going well until it reaches a certain layer, where the filament does not get deposited properly for the entire layer, only intermittently. The following layers then, of course, have the same problem and I get this failed print with these “frayed ends”. Additional attempts failed the same way at a similar layer count.

If someone has some experience with lightweight PLA (LW-PLA) and knows what can be done to solve this, I and my father would greatly appreciate the help.

Thanks in advance.

Edit: Additional info: I’m using the PrusaSlicer files from the linked page. Edit2: The printer is Prusa Mk4.

  • @sun_is_ra
    link
    English
    53 days ago

    according to manufacturer Temp should be between 230-250. Maybe try with 230 and see if it helps?

    A better option is to print a “temperature tower”

    something like that: https://all3dp.com/2/temp-tower-cura-tutorial/