Printing here with eSun PLA at 215 C on a Prusa Mini, and there are lots of hairline strings.

What’s causing those strings? Temp too low?

  • Imgonnatrythis
    link
    fedilink
    English
    arrow-up
    8
    ·
    1 year ago

    Try dehydrateding your pla first. Then try some of these other suggestions. If all else fails, these clean up really nicely with a butane blow torch.