PETG has always been more fraught than PLA for me but as of late it just looks like a mess.
I’m just trying to do calibration at this point and I’m getting this mess on the pressure advance test in Orca Slicer.
I get so much stringing, boogers, and just terrible prints. It didn’t used to be this bad. Any tips?
I’m using a Snapmaker Artisan.
How old is that spool? I use rapid PETG but I have noticed that print quality goes to shit quick when it absorbs too much moisture. Absolute garbage prints when they hit a certain point. Id crack a fresh spool to calibrate with and see if that remedies the situation.
It’s somewhat old but I keep them in dry boxes with silica beads and a hygrometer. The humidity never increased past 20% I believe. Usually stays around 15%.
Have you ever dried this filament? Silica beads won’t dry out filament, they will just keep the air in the box dry. I have definitely had to dry filament from the factory, especially PETG.
I have never dried it before, no.